Standard Test Method for Drying Shrinkage of Mortar Containing Hydraulic Cement
Automatische name übersetzung:
Standard Test Method for Trockenschwindung Mörtel mit hydraulischen Zement
NORM herausgegeben am 1.12.2009
Bezeichnung normen: ASTM C596-09
Anmerkung: UNGÜLTIG
Ausgabedatum normen: 1.12.2009
SKU: NS-14189
Zahl der Seiten: 3
Gewicht ca.: 9 g (0.02 Pfund)
Land: Amerikanische technische Norm
Kategorie: Technische Normen ASTM
Keywords:
drying shrinkage, hydraulic cement, method, mortar, Cement mortars, Change in length, Drying shrinkage, Portland cement, Shrinkage--drying, Volume shrinkage, ICS Number Code 91.100.10 (Cement. Gypsum. Lime. Mortar)
Significance and Use | ||||||||||||||||||
This test method establishes a selected set of conditions of temperature, relative humidity and rate of evaporation of the environment to which a mortar specimen of stated composition shall be subjected for a specified period of time during which its change in length is determined and designated “drying shrinkage”. The drying shrinkage of mortar as determined by this test method has a linear relation to the drying shrinkage of concrete made with the same cement and exposed to the same drying conditions. Hence this test method may be used when it is desired to develop data on the effect of a hydraulic cement on the drying shrinkage of concrete made with that cement. |
||||||||||||||||||
1. Scope | ||||||||||||||||||
1.1 This test method determines the change in length on drying of mortar bars containing hydraulic cement and graded standard sand. 1.2 The values stated in SI units are to be regarded as standard. When combined standards are referenced, the selection of measurement system is at the user’s discretion subject to the requirements of the referenced standard. 1.3 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use. (Warning—Fresh hydraulic cementitious mixtures are caustic and may cause chemical burns to skin and tissue upon prolonged exposure). |
||||||||||||||||||
2. Referenced Documents | ||||||||||||||||||
|
Wollen Sie sich sicher sein, dass Sie nur die gültigen technischen Normen verwenden?
Wir bieten Ihnen eine Lösung, die Ihnen eine Monatsübersicht über die Aktualität der von Ihnen angewandten Normen sicher stellt.
Brauchen Sie mehr Informationen? Sehen Sie sich diese Seite an.
Letzte Aktualisierung: 2024-12-23 (Zahl der Positionen: 2 217 157)
© Copyright 2024 NORMSERVIS s.r.o.