Wir benötigen Ihre Einwilligung zur Verwendung der einzelnen Daten, damit Sie unter anderem Informationen zu Ihren Interessen einsehen können. Klicken Sie auf "OK", um Ihre Zustimmung zu erteilen.
Standard Test Method for Polyurethane Raw Materials: Determination of Primary Hydroxyl Content of Polyether Polyols
Automatische name übersetzung:
Standardtestverfahren für Polyurethan-Rohstoffe: Bestimmung des Gehalts an primärem Hydroxyl von Polyetherpolyolen
NORM herausgegeben am 1.4.2011
Bezeichnung normen: ASTM D4273-11
Anmerkung: UNGÜLTIG
Ausgabedatum normen: 1.4.2011
SKU: NS-26638
Zahl der Seiten: 8
Gewicht ca.: 24 g (0.05 Pfund)
Land: Amerikanische technische Norm
Kategorie: Technische Normen ASTM
Keywords:
NMR, nuclear magnetic resonance spectroscopy, polyurethane raw materials, primary hydroxyl, polyether polyol, Hydroxyl (hydroxide ion) content, Nuclear magnetic resonance (NMR) spectrometry, Polyether polyols, Polyols, Polyurethane insulation, Polyurethane raw materials--polyols, ICS Number Code 83.080.20 (Thermoplastic materials)
Significance and Use | ||||||||
Measurements of primary hydroxyl content are useful for providing information regarding the relative reactivities of polyols. |
||||||||
1. Scope | ||||||||
1.1 Carbon-13 Nuclear Magnetic Resonance Spectroscopy (carbon-13 NMR), measures the primary hydroxyl content of ethylene oxide-propylene oxide polyethers used in preparing flexible foams. It is best suited for polyethers with primary hydroxyl contents of 10 to 90 %. 1.2 The values stated in SI units are to be regarded as standard. No other units of measurement are included in this standard. 1.3 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use. Note 1—There is no known ISO equivalent to this standard. X1.1.1 Fluorine-19 Nuclear Magnetic Resonance Spectroscopy (fluorine-19 NMR), measures the primary hydroxyl content in ethylene oxide-propylene oxide polyethers used in flexible urethane foams. It is suitable for polyethers with hydroxyl numbers of 24 to 300 and primary hydroxyl percentages of 2 to 98. |
||||||||
2. Referenced Documents | ||||||||
|
Wollen Sie sich sicher sein, dass Sie nur die gültigen technischen Normen verwenden?
Wir bieten Ihnen eine Lösung, die Ihnen eine Monatsübersicht über die Aktualität der von Ihnen angewandten Normen sicher stellt.
Brauchen Sie mehr Informationen? Sehen Sie sich diese Seite an.
Letzte Aktualisierung: 2024-12-22 (Zahl der Positionen: 2 217 000)
© Copyright 2024 NORMSERVIS s.r.o.