Wir benötigen Ihre Einwilligung zur Verwendung der einzelnen Daten, damit Sie unter anderem Informationen zu Ihren Interessen einsehen können. Klicken Sie auf "OK", um Ihre Zustimmung zu erteilen.
Standard Test Method for Determining Tearing Strength of Internally Reinforced Geomembranes (Includes all amendments And changes 6/12/2015).
Automatische name übersetzung:
Standard Test Methode zur Bestimmung der Reißfestigkeit der Innenverstärkung Dichtungsbahnen
NORM herausgegeben am 1.3.2010
Bezeichnung normen: ASTM D5884-04a(2010)
Anmerkung: UNGÜLTIG
Ausgabedatum normen: 1.3.2010
SKU: NS-32940
Zahl der Seiten: 3
Gewicht ca.: 9 g (0.02 Pfund)
Land: Amerikanische technische Norm
Kategorie: Technische Normen ASTM
Keywords:
geomembrane, reinforced, tearing strength, textile, Geomembranes, Internally reinforced geomembranes, Reinforced geomembranes, Tear testing--geosynthetic materials/applications, ICS Number Code 59.080.70 (Geotextiles)
Significance and Use | ||||||
Since tear resistance may be affected to a large degree by mechanical fibering of the membrane under stress, as well as by stress distribution, strain rate, and size of specimen, the results obtained in a tear resistance test can only be regarded as a measure of the resistance under the conditions of that particular test and not necessarily as having any direct relation to service value. This test method measures the force required to tear a reinforced geomembrane along a reasonably defined course such as that the tear propagates across the width of the specimen. The values may vary between types of reinforcement used within a geomembrane. The tongue tear method is useful for estimating the relative tear resistance of different reinforcing textiles or different directions in the same reinforcing textiles. Disputes—In case of a dispute arising from differences in reported test results when using this test method for acceptance testing of commercial shipments, the purchaser and the supplier should conduct comparative tests to determine if there is a statistical difference between their laboratories. |
||||||
1. Scope | ||||||
1.1 This test method covers a uniform procedure for determining the tear strength of flexible geomembranes internally reinforced with a textile, using the tongue tear method. 1.2 The values stated in SI units are to be regarded as the standard. The inch-pound units given in parentheses are for information only. 1.3 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use. |
||||||
2. Referenced Documents | ||||||
|
Wollen Sie sich sicher sein, dass Sie nur die gültigen technischen Normen verwenden?
Wir bieten Ihnen eine Lösung, die Ihnen eine Monatsübersicht über die Aktualität der von Ihnen angewandten Normen sicher stellt.
Brauchen Sie mehr Informationen? Sehen Sie sich diese Seite an.
Letzte Aktualisierung: 2024-11-22 (Zahl der Positionen: 2 206 568)
© Copyright 2024 NORMSERVIS s.r.o.