Wir benötigen Ihre Einwilligung zur Verwendung der einzelnen Daten, damit Sie unter anderem Informationen zu Ihren Interessen einsehen können. Klicken Sie auf "OK", um Ihre Zustimmung zu erteilen.
Standard Test Method for Determining Tensile Properties of Nonreinforced Polyethylene and Nonreinforced Flexible Polypropylene Geomembranes
Automatische name übersetzung:
Standard Test Methode zur Bestimmung der Zugeigenschaften von unverstärkten Polyethylene und Polypropylene unverstärkten Flexible Dichtungsbahnen
NORM herausgegeben am 1.6.2004
Bezeichnung normen: ASTM D6693-04
Anmerkung: UNGÜLTIG
Ausgabedatum normen: 1.6.2004
SKU: NS-36169
Zahl der Seiten: 5
Gewicht ca.: 15 g (0.03 Pfund)
Land: Amerikanische technische Norm
Kategorie: Technische Normen ASTM
Keywords:
nonreinforced, percent break elongation, percent yield elongation, polyethylene, polypropylene, tensile break strength, tensile yield strength, ICS Number Code 59.080.70 (Geotextiles)
1. Scope | ||||||||||||||
1.1 This test method covers the determination of the tensile properties of nonreinforced geomembranes in the form of standard dumbbell-shaped test specimens when tested under defined conditions of pretreatment, temperature and machine speed. 1.2 This test method can be used for testing materials thickness between 0.25 mm (0.010 in) and 6.3 mm (0.25 in.). Note 1—This test method is not intended to cover precise physical procedures. The constant rate of crosshead movement of this test lacks accuracy from a theoretical standpoint. A wide difference may exist between the rate of crosshead movement and the rate of strain of the specimen indicating that the testing speeds specified may disguise important effects or characteristics of these materials in the plastic state. Further, it is realized that variations in the thicknesses of test specimen, as permitted by this test standard, produce variations in the surface-volume ratios of such specimens, and that these variations may influence the test results. Hence, where directly comparable results are desired, all samples should be of equal thickness. Special additional tests should be used where more precise physical data are needed. 1.3 Test data obtained by this test method is relevant and may be appropriate for use in engineering design with consideration of test conditions as compared to in-service conditions. 1.4 The values stated in SI units are to be regarded as the standard. The values given in parentheses are for information only. 1.5 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use. |
||||||||||||||
2. Referenced Documents | ||||||||||||||
|
Wollen Sie sich sicher sein, dass Sie nur die gültigen technischen Normen verwenden?
Wir bieten Ihnen eine Lösung, die Ihnen eine Monatsübersicht über die Aktualität der von Ihnen angewandten Normen sicher stellt.
Brauchen Sie mehr Informationen? Sehen Sie sich diese Seite an.
Letzte Aktualisierung: 2024-11-22 (Zahl der Positionen: 2 206 568)
© Copyright 2024 NORMSERVIS s.r.o.