Standard Test Method for Multiple Stress Creep and Recovery (MSCR) of Asphalt Binder Using a Dynamic Shear Rheometer (Includes all amendments And changes 1/11/2016).
Automatische name übersetzung:
Standard Test Method for Multiple Belastungs Creep und Recovery (MSCR) von Asphalt Binder Verwendung von dynamischen Scherrheometer
NORM herausgegeben am 1.6.2010
Bezeichnung normen: ASTM D7405-10a
Anmerkung: UNGÜLTIG
Ausgabedatum normen: 1.6.2010
SKU: NS-38380
Zahl der Seiten: 4
Gewicht ca.: 12 g (0.03 Pfund)
Land: Amerikanische technische Norm
Kategorie: Technische Normen ASTM
Keywords:
asphalt binder, creep and recovery, DSR, dynamic shear rheometer, elastic recovery, MSCR, non-recoverable creep compliance, polymer modified asphalt, Asphalt binder, MSCR (multiple stress creep and recovery), Multiple stress creep and recovery (MSCR), Rheometers, ICS Number Code 91.100.50 (Binders. Sealing materials)
Significance and Use | ||||||||||||||||
This test method is used to identify the presence of elastic response in a binder and the change in elastic response at two different stress levels. Non-recoverable creep compliance has been shown to be an indicator of the resistance of an asphalt binder to permanent deformation under repeated load. This test method is also useful as a surrogate for other test methods used to measure elasticity in asphalt binders such as Test Method D5801 (Toughness and Tenacity), Test Method D6084 (Elastic Recovery), and Test Method D7175 (DSR phase angle). |
||||||||||||||||
1. Scope | ||||||||||||||||
1.1 This test method covers the determination of percent recovery and non-recoverable creep compliance of asphalt binders by means of Multiple Stress Creep and Recovery (MSCR) testing. The MSCR test is conducted using the Dynamic Shear Rheometer (DSR) at a specified temperature. 1.2 This standard is appropriate for unaged material, material aged in accordance with Test Method D2872 (RTFO), material aged in accordance with Practice D6521 (PAV), and material aged in accordance with both Test Method D2872 and Practice D6521. Note 1—The majority of development work on this test method was performed on material aged in accordance with Test Method D2872 (RTFO). 1.3 The percent recovery is intended to provide a means to determine the presence of elastic response and stress dependence of polymer modified and unmodified asphalt binders. 1.4 The values stated in SI units are to be regarded as standard. No other units of measurement are included in this standard. 1.5 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use. |
||||||||||||||||
2. Referenced Documents | ||||||||||||||||
|
Wollen Sie sich sicher sein, dass Sie nur die gültigen technischen Vorschriften verwenden?
Wir bieten Ihnen Lösungen, damit Sie immer nur die gültigen (aktuellen) legislativen Vorschriften verwenden könnten.
Brauchen Sie mehr Informationen? Sehen Sie sich diese Seite an.
Letzte Aktualisierung: 2024-12-23 (Zahl der Positionen: 2 217 157)
© Copyright 2024 NORMSERVIS s.r.o.