Wir benötigen Ihre Einwilligung zur Verwendung der einzelnen Daten, damit Sie unter anderem Informationen zu Ihren Interessen einsehen können. Klicken Sie auf "OK", um Ihre Zustimmung zu erteilen.
Standard Guide to Obtainable ASTM Equivalent Penetrameter Sensitivity for Radiography of Steel Plates 1/4 to 2 in. (6 to 51 mm) Thick with X Rays and 1 to 6 in. (25 to 152 mm) Thick with Cobalt-60 (Includes all amendments And changes 6/30/2015).
Automatische name übersetzung:
Standard-Leitfaden zur Erhältlich ASTM Equivalent Penetrameter Empfindlichkeit für Röntgenaufnahmen von Stahlplatten bis 2 1/4 in. (6-51 mm) dick mit X-Strahlen und 1 bis 6 in. (25 bis 152 mm) dick mit Kobalt-60
NORM herausgegeben am 1.7.2009
Bezeichnung normen: ASTM E592-99(2009)e1
Anmerkung: UNGÜLTIG
Ausgabedatum normen: 1.7.2009
SKU: NS-47323
Zahl der Seiten: 5
Gewicht ca.: 15 g (0.03 Pfund)
Land: Amerikanische technische Norm
Kategorie: Technische Normen ASTM
Keywords:
cobalt 60, density, equivalent penetrameter sensitivity, exposure, reference radiographic illustrations, X rays, Cobalt-60 radiography, Density, Equivalent penetrameter, Exposure tests, Penetrameters, Radiographic examination, Reference radiographs, Sensitivity criterion/response, Steel plate, X-ray monitoring/processing, ICS Number Code 77.040.20 (Non-destructive testing of metals)
Significance and Use | ||||||||||||||||||
A key consideration with any radiographic system is its capability to resolve detail (that is, sensitivity). The degree of obtainable sensitivity with a given system is dependent upon several radiographic parameters such as source energy level, film type, type and thickness of intensifying screens, exposure (density), etc. This guide permits the user to estimate the degree of sensitivity that may be obtained with X rays and cobalt-60 gamma rays when using a prescribed set of radiographic parameters. This guide may also be used in conjunction with Test Method E 746 to provide a basis for developing data for evaluation of a user's specific system. This data may assist a user in determining appropriate parameters for obtaining desired degrees of radiographic system sensitivity. An alternate to this approach is the use of those adjunct radiographic illustrations detailed in Section 6. |
||||||||||||||||||
1. Scope | ||||||||||||||||||
1.1 This guide to obtainable equivalent penetrameter sensitivity covers the minimum penetrameter thicknesses for which the image of the 1T and 2T holes is visible for a few practical radiographic conditions. The values represent near optimum sensitivity for flat steel plates. Radiographic conditions that give higher values of scatter buildup from the specimen or backscattered radiation at the image plane will give poorer sensitivity. 1.2 Eight radiographs that illustrate sensitivities obtainable with practical radiographic systems are included as adjuncts to this guide and may be obtained from ASTM. 1.3 The values stated in inch-pound units are to be regarded as the standard. The values given in parentheses are for information only. 1.4 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use. |
||||||||||||||||||
2. Referenced Documents | ||||||||||||||||||
|
Wollen Sie sich sicher sein, dass Sie nur die gültigen technischen Normen verwenden?
Wir bieten Ihnen eine Lösung, die Ihnen eine Monatsübersicht über die Aktualität der von Ihnen angewandten Normen sicher stellt.
Brauchen Sie mehr Informationen? Sehen Sie sich diese Seite an.
Letzte Aktualisierung: 2024-12-22 (Zahl der Positionen: 2 217 000)
© Copyright 2024 NORMSERVIS s.r.o.